When used as indicated in Method 1, this product will reveal the general structure of pure Platinum and Platinum alloys.

When used as described in Method 2, this product will reveal the general structure of Rhuthenium and the grain structure of Rhuthenium under polarised light.

When used as described in Method 3 this product will reveal the general structure of Indium.

 

Description

Electrolytic etch—use carbon cathode and platinum wire connection to specimen.

  1. Use 6 Volts ac for 1 minutes.
  2. Use 5 to 20 Volts ac for between 1 and 2 minutes.
  3. Use 20 Volts ac for between 1 and 2 minutes.

For etch-polishing, use shorter times.

After etching, water rinse, alcohol rinse, and dry.